Aタップ | オーエスジー

34 件中 11-20 件を表示

answer
Untitled Documents

Use of S-XPF in stainless steel

For use on stainless steel, it is recommended to use an insoluble cutting fluid or a water-soluble cutting fluid with good lubricity.

References: Cutting Data Table 



(FAQID:567)
No : 567
公開日時 : 2024/10/22 00:00 更新日時 : 2024/11/01 02:39
カテゴリー: A-tap
answer
Untitled Documents

How deep can S-XPF be drilled?

As with other grooveless Tap , first consider a depth of about 3 times the diameter of the tool. However, it may vary depending on the workpiece material.



(FAQID:568)
No : 568
公開日時 : 2024/10/22 00:00 更新日時 : 2024/11/01 02:38
カテゴリー: A-tap
answer
Untitled Documents

Do the M2.6, M3, and M4 tool materials of S-XPF contain at least 6 substances that are RoHS compliant?

S-XPF M2.6, M3, and M4 tool materials do not contain 6 substances that are RoHS compliant.



(FAQID:569)
No : 569
公開日時 : 2024/10/22 00:00 更新日時 : 2024/11/01 02:38
カテゴリー: A-tap
answer
What is the model number of the A-SFT end mill shank specification?

What is the model number of the A-SFT end mill shank specification?

There is no special model number, and it remains A-SFT. You can distinguish them by "Tool No."



(FAQID:584)
No : 584
公開日時 : 2024/10/22 00:00 更新日時 : 2024/11/01 02:38
カテゴリー: A-tap
answer
Dry processing in A<span translate="no"> Tap </span>

Dry processing at A Tap

It is okay to use insoluble cutting oil and water-soluble emulsion type, but we do not recommend water-soluble oil with poor lubricity or dry processing.

Reference:

No : 595
公開日時 : 2024/10/22 00:00 更新日時 : 2024/11/01 02:38
カテゴリー: A-tap
answer
High-efficiency machining in A<span translate="no"> Tap </span>

High-efficiency machining at A Tap

For machining with a cutting speed of 15 m/min or more, it is recommended to use a machine with a synchronous feed mechanism.



Reference:
No : 596
公開日時 : 2024/10/22 00:00 更新日時 : 2024/11/01 02:38
カテゴリー: A-tap
answer
Asynchronous machining in A<span translate="no"> Tap </span>

Asynchronous machining in A Tap

A-SFT AND A-POT can also be used in asynchronous environments.

If you are considering performance stabilization and high-efficiency machining exceeding 15 m/min, we recommend
No : 597
公開日時 : 2024/10/22 00:00 更新日時 : 2024/11/01 02:38
カテゴリー: A-tap
answer
Recommended machining depth for A<span translate="no"> Tap </span>

Recommended machining depth for A Tap

A Tap is recommended to have a machining depth of up to 2.5 times the thread diameter (2D: Dc×2.5).

Reference:

No : 598
公開日時 : 2024/10/22 00:00 更新日時 : 2024/11/01 02:38
カテゴリー: A-tap
answer
A-<span translate="no"> Tap </span>aluminum machining

A- Tap aluminum machining

A Tap supports aluminum machining. Since the chip treatment performance is excellent, it is possible to aim for stable processing compared to conventional general-purpose coating

No : 599
公開日時 : 2024/10/22 00:00 更新日時 : 2024/11/01 02:38
カテゴリー: A-tap
answer
What is the guideline for A-SFT and A-POT material hardness?

What is the guideline for A-SFT and A-POT material hardness?

The approximate material hardness (HRC) that can be processed by A-SFT AND A-POT is as follows.

 