In the processing of titanium alloys, bellows-shaped chips are emitted, which is a phenomenon that tends to occur when the cutting conditions are too fast.
Reduce the cutting speed or set the feed amount per revolution to 1.5%~2% of the drill diameter and check the chip condition.
▼ Bellows-shaped chips

References: ADO-SUS Series